Two strange happenings in the studio:
The first I need some help with is that the saline sulphate solution jellyfied, now why would that happen? It was 50/50 mix of 1kilo each salt and copper sulphate diluted with 7 litres of water. Well it was when I started it but some one else might have added to the mix.
The second is a problem with two photo polymer plates I made. The dark areas are raised above the light areas which made intaglio inking impossible. I ended up treating them as a relief prints.
Anybody reading this got any ideas?