02 April 16 P1070943 Aquatint: Step 5, Once the varnish is dry, place the plate in the acid bath for the first dunk approx 5 secs (all timings are for zinc plate and Nitric Acid 20:1 NB times for other acids and metals will vary). Rinse and dry the plate. 0 Comments